1, Nqe lus piav txog Kev Tiv Thaiv Carburizing Mullite Cib: Cov khoom lag luam yog ua los ntawm cov ntaub ntawv raw nrog kev ua kom huv siab los ntawm kev nchuav los yog Lattice nias thiab kub kub tua, Cov khoom lag luam yog hom tshiab ntawm cov khoom siv hluav taws xob, uas muaj kev tiv thaiv zoo kom txo cov roj cua xws li H2. thiab CO hauv qhov kub siab ntev
2, Daim Ntawv Thov Kev Tiv Thaiv Carburizing Mullite Cib: dav siv hauv cov pa taws ua pa taws ua kom sov, cov nplaim hluav taws kub hnyiab, cov cua sov ua kom sov, kho cua sov rauv, thiab lwm yam.
3, Yam ntxwv ntawm Kev Tiv Thaiv Carburizing Mullite Cib :
1) Fe2O3 cov ntsiab lus qis , .70.7%
2, Zoo carburizing kuj
3, Kev hloov pauv me me hauv kab ntawm kev rov them nyiaj
4, Tshuaj zoo ruaj khov
5, Tsawg thermal conductivity
6, Zoo heev yaig tsis kam
![FC5~8XSQG~Z[VIN_MBI_]@S](/Content/uploads/2021433345/20210311093851be78e30ca666476b892a130aa1012d89.png)
4, Index ntawm Anti Carburizing Mullite Cib:
ITEM | KST-0.5 | KST-0.6 | KST-0.8 | KST-1.0 |
Al2O3 % | ≥42 | ≥45 | ≥48 | ≥48 |
Fe2O3 % | ≤0.7 | ≤0.7 | ≤0.7 | ≤0.6 |
BD g/cm3 | ≤0.5 | ≤0.6 | ≤0.8 | ≤1.0 |
Lub zog txias txias Mpa | ≥1.5 | ≥2.0 | ≥3.0 | ≥4.2 |
Rov ua kom sov hloov pauv % | 1300℃×12h ≤0.5 | 1300℃×12h ≤0.5 | 1300℃×12h ≤0.4 | 1300℃×12h ≤0.4 |
Thermal conductivity w/mk 350±25℃ | ≤0.18 | ≤0.25 | ≤0.35 | ≤0.45 |
Kev pabcuam kub ℃ | ≥1300 | ≥1300 | ≥1300 | ≥1350 |
5.Qhov tswv yim zoo ntawm kev siv cov khoom lag luam, cov khoom tau raug xa tawm mus rau Russia, Tebchaws Asmeskas, Morocco
6.Peb yog tus muab khoom tshaj lij, leej twg tuaj yeem muab cov neeg siv khoom siv thev naus laus zis dawb, siv thiab lwm yam teeb meem.
Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv hluav taws xob?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawv thov hu rau peb
Tiv tauj kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAX: 86-0533-4188518
Rose: +86-13275332819 (wechat/tus lej whatsapp)
Cim npe nrov: anti carburizing mullite cib, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom