Kev Sib Txuas Hom Tin Bath Roof Blocks txais cov qauv ua ke tag nrho, uas yog tsim los ntawm choj cib module, txhawb cib module thiab ntsaws cib module. Lub ntsej muag ua haujlwm ntawm cov qauv yog sintered sillimanite cib, lub ntsej muag tsis ua haujlwm yog 2- txheej thermal rwb thaiv tsev cib, thiab lub mis phab ntsa yog mullite thermal rwb thaiv tsev cib. Nyob rau hauv txoj kev no, tsis muaj ntsug los ntawm kev sib koom ua ke ntawm sab sauv thiab qis ntawm cov qauv, uas ua kom muaj kev ncaj ncees ntawm cov qauv groove milling, txhim kho cov kev pab cuam lub neej ntawm cov qauv thiab cov khoom iav zoo.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Cov txheej txheem tseem ceeb ntawm Combined Type Tin Bath Roof Block

Yam khoom

UNIT

TECHNCIAL INDEX

Al2O3

feem pua

Ntau dua lossis sib npaug li 58

Fe2O 3

feem pua

Tsawg dua los yog sib npaug rau 1.0

R2O

feem pua

Tsawg dua lossis sib npaug rau 0.5

Qhov ntom

g/cm3

Ntau dua lossis sib npaug li 2.30

Porosity

feem pua

Tsawg dua los yog sib npaug li 20

Txias crushing zog

Mpa

Ntau tshaj los yog sib npaug rau 50

Refractoriness

degree

1790

Refractoriness nyob rau hauv load

degree

Ntau dua lossis sib npaug rau 1450

linear tus nqi hloov

1400 degree * 2h

feem pua

±0.1

Thermal shock stability

1100 degree, dej txias

sij hawm

Ntau dua lossis sib npaug 22

2, Kev piav qhia ntawm Kev Sib Txuas Hom Tin Bath Roof Block: da dej saum ru tsev, Tin da dej refractory cib muab faib ua ob hom: hauv qab cib thiab sab saum toj cib. Cov khoom siv tseem ceeb yog hluavtaws sillimanite. Cov ntxhia theem ntawm cov khoom yog feem ntau mullite theem thiab corundum theem. Nws cov kev ua haujlwm tiv thaiv stripping (1100 degree, dej txias) yog > 25 zaug, uas yog qhov zoo heev. Nws muaj qhov zoo heev los tiv thaiv alkaline cua yaig thiab alkaline kua erosion nyhuv.Kev xyaum tau ua pov thawj tias daim ntawv thov ntawm tin da dej cib nyob rau hauv loj-scale ntab iav ntau lawm kab ua tiav tiav. Kev tsim kho ntawm tin da dej cib yog ua ke, tsis muaj qhov sib txawv ntsug. Cov qauv sib dhos yog nruj heev, thiab nws yog qhov nyuaj rau huab cua ntws los yog kua kom dhau mus. Nws tsis tsuas yog ua kom lub cev ua haujlwm ntawm iav ntau lawm kab, tab sis kuj ua kom zoo ntawm cov khoom iav.Our Hoobkas muaj zoo meej thiab siab heev ntau lawm tshuab rau tin da dej cib, nrog ntau tshaj kaum xyoo ntawm kev tsim khoom. Tom qab tau thov nyob rau hauv ntau tshaj 300 cov kab ntau lawm, peb lub tuam txhab tau txais txiaj ntsig zoo los ntawm cov neeg siv khoom. Tshwj xeeb, lub Hoobkas iav hauv Iran tau siv peb cov khoom rau ntau tshaj 7 xyoo yam tsis muaj teeb meem zoo.

3, Daim ntawv thov cuam tshuam ntawm Kev Sib Txuas Hom Tin Bath Roof Block: cov qauv muaj kev ncaj ncees, kev nyab xeeb thiab kev ntseeg siab, thiab yuav tsis tsim qhov chaw tsis xws luag ntawm lub iav phaj, ua kom cov khoom zoo thiab kev nyab xeeb ntawm cov qauv. Nws tau siv ntau tshaj 300 ntab iav ntau lawm kab hauv tsev thiab txawv teb chaws, thiab tau ua tiav daim ntawv thov zoo heev

4, Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Nyiv, Pakistan

5, Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom siv khoom siv dawb, siv thiab lwm yam teeb meem





Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv refractory?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawd thov hu rau peb



Hu rau kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / Fax: 86-0533-4188518

Rose: ntxiv rau 86-13275332819(wechat/whatsapp tooj)


Cim npe nrov: ua ke hom tin da dej ru tsev thaiv, Suav teb, manufacturers, lwm tus neeg, Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall