1, Kev piav qhia ntawm Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob ru tsev prefabricated thaiv: VD lub qhov cub npog, VOD lub qhov cub npog, LF lub qhov cub npog, tundish npog, Qhov loj-scale siab aluminium prefabricated thaiv rau sab saum toj npog ntawm lub qhov cub hluav taws xob yog tsim los ntawm cov khoom siv loj loj. Cov khoom siv zoo calcining lossis electrofusion raw khoom raug xaiv, qhov tsim nyog raw khoom particle loj yog xaiv, tom qab tag nrho kev sib xyaw, cov khoom siv loj ntawm kev co molding raug xaiv, tag nrho kev co casting molding yog saws, thiab cov kub kub binder yog. ntxiv los ua kom cov khoom tsim ntau compact, siab dua qhov ntom ntawm dav dav aluminium cib. Cov khoom yog ib qho loj thaiv nrog maj mam sib dhos thiab ob peb qhov khoob. Thaum lub sij hawm siv cov khoom, qhov kub tsis kam, kub ntws yaig kuj thiab hluav taws xob tiv thaiv yog txhim kho, thiab cov spilling kuj zoo heev. Nyob rau hauv qhov kub thiab txias, cov qauv kev ua tau zoo ntawm cov khoom yog ruaj khov, thiab kev siv cov nyhuv yog siab dua li ntawm high aluminium cib masonry. Nws yog cov khoom siv hluav taws xob zoo tshaj plaws ntawm cov khoom siv hlau thiab cov nroj tsuag hlau
2, Kev ua haujlwm tseem ceeb ntawm Hluav Taws Xob Hluav Taws Xob ru tsev prefabricated thaiv
Yam khoom | UNIT | DLG-70 | DLG-90 |
Al2O3 | feem pua | >70 | >90 |
Qhov ntom | g/cm3 | 110 degree * 24h, 2.80 1500 degree * 3h, 2.75 | 110 degree * 24h, 2.95 1500 degree * 3h, 2.90 |
Linear hloov tus nqi | 1500 degree * 3h, feem pua | ±0.7 | {0}} ntxiv rau 0.5 |
Flexural zog | Mpa | 110 degree * 24h, 5 1500 degree * 3h, 15 | 110 degree * 24h, 10 1500 degree * 3h, 18 |
Compressive zog | Mpa | 110 degree * 24h, 25 1500 degree * 3h, 50 | 110 degree * 24h, 60 1500 degree * 3h, 70 |
3, Cov yam ntxwv ntawm hluav taws xob rauv lub ru tsev prefabricated thaiv:
1) Kev ncaj ncees zoo, kev tsim kho yooj yim, cov khoom yog ib qho loj prefabricated thaiv, thiab txhua yam khoom muaj qhov kub-resistant steel nuv. Tus neeg siv tsuas yog yuav tsum tau nqa txhua yam khoom rau saum lub qhov cub hluav taws xob thiab sib sau ua ke, thiab tom qab ntawd siv cov khoom siv hluav taws xob kub kub rau qhov sib txawv, uas txuag lub sijhawm thiab nrawm dua li cov thawj masonry ntawm txhua lub siab aluminium cib.
2) Muaj zog tiv thaiv arc hluav taws xob, cov khoom lag luam yog ua los ntawm cov khoom siv ua los ntawm cov khoom siv loj, phosphoric acid high-strength binder li binder, tom qab lub sij hawm ntev ntuj ziab thiab kub kub kom qhuav. Lub compactness, high-temperature kuj, arc hluav taws xob tsis kam thiab thermal shock tsis kam ntawm cov khoom yog superior rau cov thawj high alumina cib, uas yog feem ntau siv nyob rau hauv loj hlau thiab steel nroj tsuag. Tom qab sib sau ua ke, tag nrho cov qauv ntawm cov khoom yog nruj, tsis muaj kab nrib pleb thiab ntog, thiab nws cov kev pab cuam lub neej yog ntev tshaj li cov thawj high alumina cib masonry.
3) Nws muaj kev tiv thaiv zoo rau kev txias txias thiab cua sov
4) Lub zog muaj zog hauv lub xeev txias thiab lub xeev kub
5) Kev tiv thaiv rau cov hlau slag thiab kub siab airflow yaig
4, Daim Ntawv Thov: Feem ntau yog siv rau hauv hluav taws xob cua sov lub ru tsev
5, Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Russia, Pakistan
6, Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom pub dawb cov khoom siv thev naus laus zis, siv thiab lwm yam teeb meem, peb lub Hoobkas muaj ntau tshaj kaum xyoo ntawm kev tsim khoom zoo tshaj plaws thiab kev siv tshuab ntau lawm, nrog rau cov cuab yeej siv siab heev thiab cov thev naus laus zis. Peb cov khoom siv tau zoo nyob rau hauv Shougang Group Company, Baosteel tuam txhab, Shandong Hlau thiab steel tuam txhab thiab lwm yam loj-scale hlau thiab steel nroj tsuag nyob rau hauv Tuam Tshoj. Tam sim no, peb cov khoom raug xa tawm mus rau ntau lub teb chaws, txais tos cov neeg siv khoom thiab cov phooj ywg los tham thiab sib pauv
Koj puas xav nrhiav tus kws tshaj lij ntawm Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob ru tsev prefabricated thaiv?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: ntxiv rau 86-13275332819(wechat/whatsapp tooj)
Cim npe nrov: Electric Rauv Roof Prefabricated Block, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom