1, Kev piav qhia ntawm Magnesite-Ferrum-alumina Spinel Brick:
Cov khoom no tshwj xeeb tshaj yog siv rau hauv cov txheej txheem qhuav ntawm cov cement kiln, hloov lub qub magnesia cib, magnesia-alumina spinel cib, cov nyhuv ntawm cov txheej txheem tiv thaiv yog zoo heev, muaj zog hnav tsis kam, muaj zog anti-spalling kev ua tau zoo, muaj zog tiv thaiv alkali corrosion. kev ua tau zoo, thiab nws cov kev pab cuam lub neej yog pom tseeb siab dua li ntawm cov khoom siv hloov. Cov khoom no kuj siv nyob rau hauv non-ferrous hlau smelting industrial furnaces.
2, Index ntawm Magnesite-Ferrum-alumina Spinel Brick:
Yam khoom | JMFA Spinel Cib |
MgO feem pua | Ntau dua lossis sib npaug li 80 |
Fe2O3 feem pua | Ntau dua lossis sib npaug rau 4-8 |
Al2O3 feem pua | 5-10 |
Pom tseeb porosity feem pua | 17 |
Qhov ntom ntom g / cm3 | 2.9 |
Txias crushing zog Mpa | 50 |
Refractoriness nyob rau hauv load degree | 1650 |
Thermal conductivity (350 ± 25 degree) w / (mk) | 3.5 |
Thermal shock resistance, lub sij hawm | 30 |
3, Magnesite-Ferrum-alumina Spinel Brickof characteristics:
1) Cov khoom lag luam yog cov khoom sib xyaw spinel cov khoom siv nrog cov qauv compact heev.tom qab siv hauv cov cement rotary kiln, cov nyhuv ntawm kev tsim cov txheej txheem tiv thaiv zoo heev thiab kev pab cuam lub neej ntawm lub kiln yog ntev heev. cov khoom muaj zoo heev corrosion kuj rau alkali slag.
2) Cov khoom yog alkaline refractory cib tsim nyob rau hauv xyoo tas los no rau cov cement kilns loj, uas hloov cov magnesia-alumina spinel cib yav dhau los thiab txhim kho kev ua haujlwm ntawm cov cement kilns.
3) Cov khoom muaj qhov loj shaping siab, siab sintering kub thiab me me dimension kam rau ua.
4, Cov khoom ntim:
siv kev nyab xeeb, ruaj khov thiab noo noo-pov thawj packing haum rau kev thauj mus los hauv av thiab hiav txwv
5, Peb qhov kev pabcuam:
1) Muab cov lus qhia pub dawb rau cov neeg siv
2) Pub dawb rau cov neeg siv los muab cov lus piav qhia ntawm cov khoom siv
3) Dawb rau cov neeg siv los muab cov khoom tsim qauv tsim qauv
4) Dawb rau cov neeg siv los muab cov qauv, rau cov neeg siv kev sim
6, Peb qhov zoo:
1) Kev tshaj lij, nrog ntau tshaj 20 xyoo ntawm kev tsim khoom thiab kev lag luam, muaj zog sib pauv thiab kev pabcuam
2) Peb muaj peb tus kheej Refractory cov khoom tsim kev koom tes Hoobkas
Khoom siv lus dab neeg



![C]SZCXHD)VGENF@UQK81[12](/Content/uploads/2021433345/202101271044265e0f4a2b2ed946b7a85998b1496291e0.png)

7.Cov lus pom zoo ntawm cov khoom siv, cov khoom tau raug xa tawm mus rau Russia, Oman, Tebchaws Meskas, Kenya, Mexico
8.Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom siv khoom siv dawb, siv thiab lwm yam teeb meem.
Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv refractory?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: ntxiv rau 86-13275332819(wechat/whatsapp tooj)
Cim npe nrov: magnesite-ferrum-alumina spinel cib, Suav teb, manufacturers, lwm tus neeg, Hoobkas, siv, khoom