Magnesium Aluminium Carbon Bricks Rau Ladle

Magnesium Aluminium Carbon Bricks Rau Ladle

Magnesium Aluminium Carbon Bricks Rau Ladle yog cov cib ua hluav taws xob txhim kho los ntawm cov txheej txheem magnesia carbon cib ntau lawm. Magnesia alumina carbon cib muab los ntawm peb lub tuam txhab tau ua ob qhov kev txhim kho loj. Ua ntej, kev tiv thaiv ib puag ncig yog siv los ua phau ntawv los ua kom cov khoom lag luam zoo dua ib puag ncig thiab txuag hluav taws xob. Thib ob. Qhov ntsuas kub tau nce mus rau 300 ° C ± 20 ° C, yog li cov khoom muaj qhov pom pom qis dua, muaj zog siab dua thiab muaj zog tiv taus slag tiv taus. Cov khoom lag luam yog cov khoom tsim nyog hauv chav kawm nrog hom TRR.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Kev Ntsuas:

Yam khoom

Index

MgO %65
Al2O3 %15
C %14
SIB 2 %1.7
Fe2O3 %1.0
CaO %
1.3

Porosity %

3.5

Txias zuaj lub zog Mpa

62

BD g/cm3

3.05

2, Kev Paub Txog Magnesium Aluminium Carbon Bricks Rau Ladle:Raws li cov khoom ib txwm ua ntawm magnesia-alumina-carbon bricks, ob qhov kev txhim kho loj tau ua tiav.one yog hloov cov ntawv ib txwm tso rau hauv ib puag ncig tiv thaiv hom cawv-raws binder, qhov thib ob yog hloov cov tsoos ci kub los ntawm 200 ℃ 20 txog 300 ± ± 10, qhov kev txhim kho no muaj cov hauv qab no zoo dua li cov khoom lag luam ib txwm muaj. 1: nrog kev hloov pauv ntawm phau ntawv, cov khoom tau dhau los ua ib puag ncig tiv thaiv cov khoom lag luam uas yog qhov tsis muaj tshuaj lom thiab tsis muaj teeb meem. cov khoom tau txhim kho kev ua haujlwm ib puag ncig zoo heev, thiab cov neeg siv muaj kev tshuaj xyuas zoo ntawm nws. 2: nrog kev nce ntawm qhov kub thiab txias, qhov ntom ntom, porosity thiab lub zog ntawm cov khoom zoo dua li cov khoom lag luam ib txwm muaj, yog li txhim kho kev siv cov khoom lag luam .users txaus siab heev nrog ob qho kev txhim kho no.

3, Daim Ntawv Thov ntawm Magnesium Aluminium Carbon Bricks Rau Ladle:ladle, hluav taws xob cua sov, tsheb torpedo, hloov pauv, thiab lwm yam.

Peb qhov zoo hauv kev tsim cov magnesia carbon bricks: magnesia carbon bricks siv hauv kev hloov pauv thiab cov khoom siv tsim los ntawm peb lub Hoobkas txawv ntawm cov khoom siv magnesia carbon cib. Qhov sib txawv loj tshaj plaws yog:

1) Ib puag ncig-phooj ywg cawv raws cov ntaub ntawv yas tau siv. Qhov porosity ntawm cov khoom qis dua li ntawm cov khoom lag luam ib txwm muaj, tus qauv tus nqi yog%4%, ntsuas tus nqi yog 3.2-3.5%, thiab lub zog nrawm yog siab dua li ntawm cov khoom ib txwm muaj, tus qauv tus nqi yog MP 40MPa , ntsuas tus nqi yog 45-65mpa. Yog li ntawd, cov khoom muaj qhov ua kom zoo dua qub, ua kom zoo dua qub thiab ua kom sov ntau dua.

2) Siv 280-320 ℃ kub kub ci, cov khoom tsis muaj tshuaj lom thiab tsis qab nyob hauv cov txheej txheem cua sov, thiab muaj kev phom sij me ntsis rau ib puag ncig ib puag ncig thiab tib neeg lub cev, uas ua tau raws li qhov xav tau ntawm cov khoom tiv thaiv ib puag ncig. Ib qho ntxiv, peb lub tshuab tsim khoom lag luam yog qhov zoo tshaj plaws, cov cuab yeej ua khoom loj thiab zoo dua, cov cuab yeej kuaj sim ua tiav, lav tag nrho cov kev xav tau ntawm cov khoom, tam sim no, cov khoom lag luam hauv tsev thiab txawv teb chaws cov neeg siv tau txais kev tshuaj xyuas zoo, siv cov txiaj ntsig zoo dua li cov khoom ib txwm muaj

4, Khoom ntim:Thermal shrinkable zaj duab xis ntim ntim, pov thawj dej noo, ruaj, yooj yim thauj thiab tiv thaiv cov khoom los ntawm kev puas tsuaj.

5, Yam puas tsuaj hauv daim ntawv thov khoom:

1) Slag hauv cov hlau molten reacts nrog cov khoom ntawm qhov kub thiab txias, ua rau xoob ntawm cov qauv khoom, yaig qhov los yog spalling.

2) Qhov cuam tshuam ntawm cov hlau yaj rau ntawm cov khoom

3) Qhov kub thiab txias ntawm cov hlau yaj tau muaj qhov cuam tshuam rau saum npoo thiab cov qauv sab hauv ntawm cov khoom.

6, Txog peb kev tsim khoom thiab muab khoom ntawm cov khoom no:raws li tus neeg siv' qhov xav tau, peb lub Hoobkas tau txhim kho hauv cov txheej txheem tsim khoom qub, yog li cov khoom lag luam muaj kev ua tau zoo dua qub.Ua piv txwv li, qhov ntom ntom nce ntxiv, lub zog nce, qhov porosity qis dua, thiab ib puag ncig kev ua masonry tau zoo dua, yog li cov khoom ua tau raws li tus neeg siv' qhov xav tau thiab tau txais txiaj ntsig zoo. Tam sim no, kev tiv thaiv ib puag ncig magnesia-alumina-carbon cib ua los ntawm peb lub Hoobkas tsis tsuas yog muab cov hlau loj hauv tsev, tab sis tseem xa tawm mus rau Australia, Lub Tebchaws Yelemees, Tebchaws Askiv, Brazil thiab lwm lub tebchaws.




1

~ZHECX%)V2%}5GKG49QP2[C



7.Qhov tswv yim zoo ntawm kev siv cov khoom lag luam, cov khoom tau raug xa tawm mus rau Oman, Tebchaws Asmeskas, Morocco thiab Is Nrias teb.

8.Lub chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov ntaub ntawv ntsuas ntsuas khoom tiav lossis cov ntawv xeem thib peb.



Tiv tauj kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat/tus lej whatsapp)




Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv hluav taws xob?

Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?

Tom qab ntawv thov hu rau peb


Tiv tauj kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat/tus lej whatsapp)


Cim npe nrov: magnesium aluminium carbon bricks rau ladle, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall