1.Txoj kev ntsuas qhov ua tau zoo ntawm Silicon Carbide Cib rau Electrolytic Aluminuim Rauv
TSWV YIM | UNITIT | JCS-1 | JCA-2 |
SIC | % | ≥87 | ≥85 |
SIO2 | % | 8 | 3 |
Al2O3 | % | --- | ≥10 |
Fe2O3 | % | ≤1.0 | ≤1.0 |
Porosity | % | ≤18 | ≤18 |
Tso Nyuaj Siab | g / cm3 | ≥2.65 | ≥2.55 |
Hlob lub zog | Mpa | ≥80 | ≥85 |
Refractoriness hauv qab ntsaws | ℃ | ≥1600 | ≥1550 |
Thermal poob siab ruaj khov, 950 ℃, cua txias | sij hawm | ≥40 | ≥35 |
Coefficient ntawm tshav kub conductivity | w/m.k | ≥8 | ≥6 |
2. Cov yam ntxwv:
1) Zoo hnav tsis kam
2) Muaj zog tiv thaiv corrosion, tsis lo-aluminium, tsis muaj slag
3) Muaj lub zog siab, muaj zog thermal conductivity
4) Zoo thermal poob siab ua haujlwm
3. Daim ntawv thov: aluminium melting rauv, lub tshuab ua kom sov, cua sov ua kom sov
4.Txhais cov lus pom zoo ntawm cov khoom lag luam tau siv, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Nyiv, Pakistan, Russia, Australia, Oman, Tebchaws Asmeskas, Kenya, Mexico, Morocco thiab Is Nrias teb.
5.Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom lag luam thev naus laus zis dawb, siv thiab lwm yam teeb meem.
Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom lag luam refractory?
Koj puas xav nrhiav tus kws tshaj tawm cov khoom hluav taws xob graphite?
Koj puas xav nrhiav tus neeg xa khoom kom ruaj khov thiab lees paub?
Tom qab ntawd cia' s kev sib cuag nrog jinggan tuam txhab
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAX: 86-0533-4188518
Rose: +86-13275332819 (wechat / whatsapp tooj)
Cim npe nrov: silicon carbide cib rau electrolytic aluminuim rauv taws ua kom sov, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, vaj tse