Siab Alumina Ceramic Fiber Board

Siab Alumina Ceramic Fiber Board

High alumina ceramic fiber board tseem hu ua aluminium silicate fiber board, uas yog ib yam ntawm cov tawv tawv tawv fiber ntau rwb thaiv tsev cua sov thiab cov khoom tiv taus hluav taws. Cov khoom siv polished muaj cov nplaim du, qhov loj me thiab lub zog siab, tab sis nws yooj yim rau txheej txheem thiab tsim. Cov khoom tsis muaj asbestos, kev tiv thaiv ib puag ncig, siv sijhawm ntev ntawm qhov kub ntawm 1000-1300 ℃, hom TRR.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Index ntawm High Alumina Ceramic Fiber Board:

Yam khoom

JST-HY602

JHP-HY603

JHA-HY604

Al2O3 %

46

47-49

52-55

Al2O3+SiO2 %

97

99

99

Na2O + K2O %

1.0

0.2

0.2

Kev faib tawm kub ℃

1260

1260

1400

Ua haujlwm kub ℃

1000

1100

1260

Tej ntom ntom kg/m3

280-350

280-350

280-350

Hloov pauv mus tas li % (220KG/m3)

1000℃×24h

-3

1100℃×24h

-3

1260℃×24h

-3

Cov cua sov ua kom sov W/M · K (260KG/m3)

400℃ 0.085

800℃ 0.132

1000℃ 0.180

400℃ 0.085

800℃ 0.132

1000℃ 0.180

400℃ 0.085

800℃ 0.132

1000℃ 0.180

Crushing zog Mpa (Nyuaj tuab 10%)

0.5

0.5

0.5

U4(1}4TL)VI0LL[G]HZKO~X


2. Cov yam ntxwv ntawm High Alumina Ceramic Fiber Board

1) Tsis muaj peev xwm ua kom sov, tsis muaj cua sov ua kom sov

2) Lub zog muaj zog siab thiab zoo toughness

3) Qhov loj me me thiab zoo du

4) Homogeneous qauv, yooj yim rau tshuab thiab teeb tsa

5) Zoo heev thermal poob siab kuj

3. Scope ntawm daim ntawv thov High Alumina Ceramic Fiber Board

1) Cov cua sov rwb thaiv tsev ntawm cov cement kiln

2) Cov cua sov rwb thaiv tsev ntawm cov nplaim hluav taws xob

3) Cov cua sov rwb thaiv tsev ntawm cov khoom siv hluav taws xob thiab cov hlau ua hlau

4) Rwb thaiv tsev kub ntawm iav qhov cub

5) Thaum tshav kub kub rwb thaiv tsev ntawm cov cua sov tsim rau txhuas smelting

6) Rwb thaiv tsev cua sov cua sov kho cua sov

4. Cov txheej txheem tsim khoom

1) Npaj cov slurry: cov paj rwb fiber ntau ceramics, muab tub lim thiab phau ntawv sib xyaw ua ke kom tsim nyog ua cov slurry.

2) khaws cov nqus: ua lub tshuab nqus tsev kom cia cov nqus nqus nqus thiab nqus dej ntau dhau

3) Kev sib sau ua ke: Nias dej kom txo cov tuab thiab nce peev txheej.

4) Kom Qhuav: Muab cov ntaub qhwv tso rau hauv cov khoom kom qhuav kom qhuav thiab tshem tawm cov dej noo.

5) Machining: Ua cov slab qhuav rau hauv cov khoom ntawm ntau yam tshwj xeeb

5, High Alumina Ceramic Fiber Board Classification:

Raws li qhov ntsuas kub ua haujlwm ntawm cov khoom, nws tuaj yeem faib ua peb pawg, JST-HY602, JSP-HY603, JHA-HY604, qhov kub ua haujlwm yog feem ntau 1000 ℃, 1100 ℃, 1260 ℃.

6, Tsis muaj asbestos hauv cov khoom, nws tsis muaj tshuaj lom, tsis qab thiab tsis muaj mob. Nws tsis muaj kev phom sij rau tib neeg lub cev thiab ib puag ncig.

7.Qhov zoo tswv yim ntawm kev siv cov khoom lag luam, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Morocco thiab Is Nrias teb.

8.Lub chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov ntaub ntawv ntsuas ntsuas khoom tiav lossis cov ntawv xeem thib peb.



Koj puas xav nrhiav tus kws tshaj lij ntawm High Alumina Ceramic Fiber Board?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawv thov hu rau peb


Hu rau kuv: Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat/tus lej whatsapp)


Cim npe nrov: siab alumina ceramic fiber board, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall