Zirconium Muaj Ceramic Fiber Board

Zirconium Muaj Ceramic Fiber Board

Zirconium Muaj Ceramic Fiber Board tseem hu ua 1400 degree aluminium silicate fiberboard, hais txog cov ceramic fiber board uas nws ua haujlwm kub txog 1400 degree. Txhawm rau txhim kho qhov hluav taws kub thiab kev pabcuam kub ntawm cov khoom, zircon raw khoom yog ntxiv raws li cov txheej txheem ntawm aluminium silicate fiberboard, kom cov ntsiab lus ntawm ZrO2 nce mus txog 15-18%, thiab qhov kev pabcuam kub yog 1400 degree. , cov khoom yog asbestos dawb, tsis muaj tshuaj lom, tsis qab, ib puag ncig-phooj ywg thiab kub resistant. Nws yog thawj cov khoom tsim nyog.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Kev piav qhia ntawm Zirconium Muaj Ceramic Fiber Board:
Cov txheej txheem ntau lawm ntawm zirconium-muaj ceramic fiber board nrog ZrO2 hmoov yog tib yam li high-alumina ceramic board.Txawm li cas los xij, kev ua haujlwm kub ntawm cov khoom tau siab dua tom qab ntxiv rau ZrO2 hmoov, thiab ncav cuag 1400 degree, lub zog ntawm cov khoom yog siab dua thiab lub toughness yog ntau dua.Cov khoom muaj qhov kub thiab txias kev ua tau zoo, xws li kev ua haujlwm ruaj khov, zoo dua lub zog thiab toughness, thiab zoo dua tiv thaiv cua yaig ntawm qhov kub thiab txias.Cov khoom siv dav siv hauv metallurgical industrial furnaces, ceramic high temperature furnaces. , chav kuaj kub kub rauv, tsis yog hlau smelting furnaces, petrochemical decomposition furnaces, thiab lwm yam., nrog rau kev pab cuam zoo dua thiab lub neej.



20QVFB(HSDF8KSB`A2RUU6F

2, Index ntawm Zirconium Muaj Ceramic Fiber Board:

Yam khoom

JZA-HY605

Al2O3%

32-33

Al2O3+SiO2 %

>80

ZrO2%

17-18

Na2O + K2O%

0.2

Classification kub degree

1400

Ua haujlwm kub degree

1360

Qhov ntom ntom kg / m3

280-350

Kev hloov pauv mus tas li % (220KG / m3)

1360 degree × 24h, 3

Thermal conductivity W/M·K (260KG/m3)

400 degree 0 085  800 degree 0.132 1000 degree 0.180

Crushing zog Mpa
(Compress thickness 10%)

0.5

3, Cov yam ntxwv ntawm Zirconium muaj Ceramic Fiber Board:

1) Raws li qhov ntev, dav thiab tuab ntawm cov khoom, nws tau muab faib ua ntau qhov tshwj xeeb thiab qhov ntau thiab tsawg, uas tuaj yeem hloov kho raws li qhov xav tau ntawm cov neeg siv, qhov ntau thiab tsawg yog 900 * 600 * 25 (50) hli.
2) Zirconium uas muaj Ceramic Fiber Board yog tsis muaj tshuaj lom, saj, tsis muaj kuab paug, board-shaped, carton-packed, thiab tuaj yeem txiav thiab siv arbitrarily.

4, Peb lub tuam txhab cog lus rau cov neeg siv khoom: los muab kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.

5, Kev Ua tiav tau tsim: Peb lub tuam txhab yav dhau los tau xa 130 tons rau Mexico.



Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv fiber ntau ceramic?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawd thov hu rau peb


Hu rau kuv: Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / Fax: 86-0533-4188518

Rose: +86-13275332819(wechat/whatsapp tus xov tooj)


Cim npe nrov: zirconium uas muaj ceramic fiber board, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall