1, Main technical parameters ntawm cov khoom
Yam khoom | UNIT | TECHNCIAL INDEX |
SIB 2 | % | 48-51 |
Al2O3 | % | 50-65 |
MgO | % | 2-5 |
Fe2O 3 | % | Tsawg dua lossis sib npaug rau 0.5 |
Na2O | % | Tsawg dua lossis sib npaug rau 0.5 |
K2O | % | Tsawg dua lossis sib npaug rau 0.5 |
Tshwj xeeb kub muaj peev xwm | kj/kg | 920-1200 |
Lub ntiajteb txawj nqus tshwj xeeb | g/cm3 | 1.2 |
Anti kub kub | degree | 500 |
Coefficient ntawm tshav kub conductivity | w/m.k | Ntau dua lossis sib npaug rau 1.25 |
Acid kuj | % | Ntau dua lossis sib npaug li 99 |
Kev nqus dej | % | Tsawg dua los yog sib npaug li 15 |
Kev pabcuam kub | degree | 1450 |
2, Kev qhia tshwj xeeb: 1{{10}}0*100*100,100*100*150,150*150*100, phab ntsa thickness:0.5,0.7,1,2,2.5*2.5,3*3,5 * 5 hexagon qhov thiab puag ncig lub qhov
3, Nta thiab kev ua haujlwm:
1) Txo cov cua kub poob ntawm cov pa tawm thiab txhim kho kev siv roj
2) Ua kom kub combustion, txhim kho combustion tej yam kev mob thiab nthuav daim ntawv thov ntawm tsawg calorific nqi roj
3) Txhim kho qhov kev sib hloov cua sov ntawm lub cub tawg, ua kom cov khoom tsim tawm thiab cov khoom zoo ntawm cov khoom siv
4) Txo cov pa pa tawm thiab cov pa phem pa tawm ntawm cov khoom siv thermal thiab txo cov pa phem
4, Daim ntawv thov teb: tshuaj nroj tsuag, smelter, fais fab nroj tsuag, boiler, tawg rauv, khib nyiab kho thermal khoom
5, Kev qhia tshwj xeeb: 100 * 100 * 100, 100 * 150 * 150, 150 * 150 * 150, 150 * 150 * 300, Tus lej ntawm qhov: 25 * 25,40 * 40,43 * 43,50 * 50,60 * 60
6, Peb lub tuam txhab cog lus rau cov neeg siv khoom: muab cov kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.
7, Kev Ua tiav tau tsim: Peb lub tuam txhab tau xa tawm yav dhau los 50-200 tons rau Kaus Lim Kauslim.
Koj puas xav nrhiav tus kws tshaj lij ntawm Mullite-corundum Honeycomb Ceramic khoom?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: mullite-corundum honeycomb ceramic, Tuam Tshoj, tuam ntxhab, lwm tus muag khoom, Hoobkas, siv, khoom