Tsev > Xov xwm > Ntsiab lus

Lub Refractory Brick Press pab txhim kho cov khoom siv refractory

Feb 26, 2026

Lub refractory cib xovxwm pab txhim kho cov ntaub ntawv refractory

Lub refractory cib xovxwm yog dav siv nyob rau hauv refractory khoom siv nyob rau hauv Tuam Tshoj, nrog zoo xws li siab automation, high efficiency, tsawg zog siv, thiab multifunctionality. Nws muaj peev xwm txhim kho tau zoo thiab kev cia siab rau kev ua lag luam zoo, thiab yog lub siab -cov khoom siv refractory cib xovxwm txhawb nqa thiab siv los ntawm lub tebchaws.
Kev tsim cov txheej txheem ntawm refractory cib xovxwm:

1. Cov khoom siv raw: Cov khoom siv raw rau cov khoom siv refractory cib (xws li silica, av nplaum, siab alumina pob zeb, magnesite, thiab lwm yam) feem ntau yuav tsum tau txais txiaj ntsig zoo, crushing, thiab tshuaj xyuas kom ua tau raws li cov txheej txheem tsim khoom ntawm cov ntaub ntawv raw ua ntej lawv tuaj yeem tsim tsim nyog.
2. Cov khoom xyaw: Ntau yam khoom siv raw rau kev tsim cov pob zeb refractory yog ntsuas thiab sib faib raws li qhov tsim nyog, thiab cov khoom siv raw zoo yog tsim los ntawm kev ntxiv ib feem ntawm cov dej los yog lwm yam binders.
3. Kev sib xyaw: Cov khoom siv raw khoom zoo sib xyaw yog sib xyaw kom zoo thiab sib xyaw ua ke nyob rau hauv qhov kev txiav txim ntawm lub log zeb kom ua tiav cov khoom zoo ib yam.
4. Moulding: Cov ntaub ntawv raw khoom npaj tau ua tiav rau hauv cov pob zeb refractory ntawm ib qho loj, cov duab, thiab lub zog los ntawm siab - siab molding siv lub tshuab cib hydraulic.
5. Drying: Muab qhov tsim refractory cib dawb paug rau ziab kom nws lub zog, ua kom cov kiln loading, thiab pab txhawb kev ua tiav ntawm cov txheej txheem sintering tom ntej.
6. Kev kub hnyiab: thauj cov cib qhuav rau hauv lub qhov cub rau sintering thiab kho, txhawm rau txhim kho lub zog compressive thiab flexural zog ntawm cov cib.
7. Kev tshuaj xyuas: Tom qab cov cib refractory raug rho tawm haujlwm los ntawm lub qhov cub, lawv tau raug kuaj xyuas cov khoom tiav thiab tsuas yog tuaj yeem ua ntau yam -tsim tom qab tau lees paub tias tsim nyog
& Cov khoom tiav warehousing: Cov khoom tsim nyog raug thauj mus rau cov khoom tiav warehouse kom tiav tag nrho cov kev tsim khoom. Cov khoom tsis raug yuav tsum tau xa rov qab mus rau * * txheej txheem rau kev ua cov khoom siv raw.