Kev sib txuas ncaj qha yog hais txog kev sib txuas ntawm cov khoom sib txuas ncaj qha nrog cov khoom. Direct bonded magnesia chrome cib yog tsim los ntawm cov txheej txheem no. Nws yog tsim los ntawm ultra-siab kub sintering nrog high-purity magnesia thiab chromium mloog zoo nrog tsawg silicon, piv txwv li SiO2<>
Qhov sib txuas ncaj qha magnesia chrome cib muaj tsawg impurities, lub iav theem yog nyob rau hauv lub triangular cheeb tsam ntawm lub crystalline theem, thiab lub toj roob hauv pes theem yog ncaj qha ua ke nrog lub crystalline theem. Nws muaj cov yam ntxwv zoo kawg nkaus ntawm qhov tsis muaj porosity, siab compressive zog, muaj zog hnav tsis kam, corrosion kuj, thermal poob siab tsis kam thiab spalling kuj.
Kev sib txuas ncaj qha magnesia chrome cib yog dav siv hauv hluav taws xob arc rauv, steel-ua hluav taws xob rauv, tawm ntawm qhov cub refining thiab cement rotary kiln.