Cordierite Mullite Shed Board Nrog Kev Pabcuam Kub Ntawm 1280 ℃

Cordierite Mullite Shed Board Nrog Kev Pabcuam Kub Ntawm 1280 ℃

Lub cordierite mullite los ua pawg nrog 1280 ℃ muaj lub zog khoov siab, uas tuaj yeem ua rau cov khoom lag luam tsawg dua 1000mm. Nws cov duab suav nrog cov laug cam, cov laug cam thiab tus ncej. Cov hom suav nrog TRR-FON, TRR-FAC, txhua yam yog cov khoom lag luam qib 1. Lub ntsiab siv lead ua tseem ceeb ntawm mullite cordierite shed phaj yog mullite, uas feem ntau siv nyob rau hauv txhua hnub ceramics, huv si ceramics, qhov cub tawg thiab lub qhov cub shuttle rau hluav taws xob cov plooj (porcelain) ntau lawm.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Cov khoom lag luam ntsuas ntawm Activated Alumina pob

ITEM

UNIT

TECHNICALIDNEX

Al2O3

%

36-39

SIB 2

%

50-52

MgO

%

7.0-8.0

Ceev

g/cm3 yog

1.82-1.85

Porosity

%

28-29

20 ℃ Flexural zog

Mpa

12-16

20 ℃ -1000 ℃ Coefficient ntawm kev nthuav dav

10-6 k-1

2.2-2.6

1250 ℃ Flexural zog

Mpa

10-11

20 ℃ cov cua sov tshwj xeeb

Kj/kg.k

1.0

Qhov kub siab tshaj plaws kev pabcuam

℃

1300

Hom


FON FAC

2, Cov yam ntxwv ntawm Cordierite mullite shed board

1) Mullite siv lead ua theem ntawm cov khoom yog ntxhib, yog li nws muaj peev xwm tiv thaiv kev deformation muaj peev xwm, muaj peev xwm loj thiab siv sijhawm ntau

2) Cov khoom lag luam muaj ntau yam, cov phaj poob thiab cov khoom txhawb nqa cov khoom sib txawv, daim ntawv thov tau nthuav dav

3) Kub siab, mus txog 1280 ℃, yog cov khoom nyiam

3, Daim Ntawv Thov: siv hauv qhov cub tawg, lub qhov cub rauv taws, lub qhov cub ci ntsa iab, cov khoom siv niaj hnub, cov khoom siv huv huv thiab cov khoom siv hauv tsev

4, Cov lus tawm tswv yim zoo ntawm cov khoom siv cuam tshuam, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Nyiv Pooj, Pakistan

5, Peb yog tus kws tshaj lij, uas tuaj yeem muab cov neeg siv khoom siv thev naus laus zis khoom siv dawb, siv thiab lwm yam teeb meem




Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv hluav taws xob?


Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv hluav taws xob graphite?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawd cia' tiv tauj nrog jinggan tuam txhab


Tiv tauj kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat/tus lej whatsapp)


Cim npe nrov: cordierite mullite shed board nrog kev pabcuam kub ntawm 1280 ℃, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom

Xa kev nug