Acid-resisting Cib Rau Chimney

Acid-resisting Cib Rau Chimney

Acid-resisting Cib Rau Chimney yog ua los ntawm cov av nplaum thiab av nplaum ua cov khoom siv tseem ceeb, los ntawm kev sib xyaw, molding, tua thiab lwm yam txheej txheem los tsim cov khoom tiv taus acid. Cov khoom muaj cov kua qaub ua haujlwm siab thiab tsis yooj yim rau oxidized hauv qhov kub ib txwm muaj. Dhau li ntawm hydrofluoric acid thiab thermal phosphoric acid, nws muaj cov tshuaj tiv thaiv zoo heev rau ntau cov tshuaj kua. Nws yog siv dav hauv hluav taws xob hluav taws xob, hlau thiab lwm yam chim chim thiab nplaim taws.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1.Feature ntawm Acid-resisting Cib Rau Chimney:

1) Cov kua qaub ua haujlwm siab, ≥ 97%, tiv thaiv xeb zoo rau feem ntau cov khoom kua qaub

2) Hloov ntim me me, tiv taus xeb zoo

3) Xim yog Ntshav liab

2. Daim ntawv thov: chimney, flue hauv ob sab phlu. Ib qho ntxiv, nws tau siv hauv cov cuab yeej tiv thaiv kab mob ntawm cov roj av, kev lag luam tshuaj lom neeg, tshuaj lom neeg thiab lwm yam lag luam.

Lub hauv paus tseem ceeb ntawm cov kua qaub -resistant cib yog SiO2, uas tsim ntau polyaluminal Andalusite nyob rau hauv tus txheej txheem ntawm kub kub sintering. Nws yog ib yam khoom uas muaj cov kua qaub ua haujlwm siab. Cov kua qaub tiv taus cov cib muaj cov qauv sib cog (ntom ≥ 2.4g/cm3), nqus dej tsawg, thiab tuaj yeem tiv taus qhov nruab nrab ntawm cov kua qaub nruab nrab ntawm chav sov. Cov khoom lag luam tau muab faib ua cov cib hnyav thiab lub teeb cib, ob qho tib si muaj cov kua qaub tiv taus huab cua, huab cua yaig thiab yaig tau zoo. Lawv tau siv dav hauv nplaim taws, chimney, coking rauv thiab cov cua sov ua tshuaj lom

3. Cov cim ntsuas kev ua tau zoo

ITEM

Chav nyob

Hnyav zoo acid acid cib TN-1

Lub teeb zoo acid tiv taus cib TN-2

SIB 2 %

%

≥55

≥65

Ceev

g/cm3 yog

2.4

1.0-1.3

Refractoriness

℃

≥1580

≥1400

Lub zog loj

Mpa

≥35

≥8

Dej nqus dej

%

≤9

≤15

Acid kuj tus nqi

%

≥98

≥97

Kev pabcuam kub

℃

1000

600

4. Cov khoom lag luam tau siv dav hauv cov pa taws loj, cov nplaim taws thiab cov cub tawg hauv Suav teb thiab xa tawm mus rau Sab Hnub Tuaj Asia thiab lwm lub tebchaws

5. Peb lub tuam txhab pub dawb los muab cov neeg siv khoom siv thev naus laus zis, siv thiab lwm yam kev pabcuam




J_CP)C5LAXURU%M`)PMJQWE




6.Qhov zoo tswv yim ntawm kev siv cov khoom lag luam, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Nyiv Pooj, Morocco

7.Peb yog tus muab khoom tshaj lij, leej twg tuaj yeem muab cov neeg siv khoom siv thev naus laus zis dawb, siv thiab lwm yam teeb meem.



Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv hluav taws xob?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawv thov hu rau peb


Tiv tauj kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat/tus lej whatsapp)


Cim npe nrov: acid-resisting cib rau chimney, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall