1, Kev piav qhia ntawm Hnav Resistant High Alumina Brick:
Cov khoom tau muab faib ua txheej hnav-resistant thiab lub teeb rwb thaiv tsev txheej. Cov txheej hnav-tiv taus muaj cov yam ntxwv ntawm qhov kub thiab txias tsis kam, hnav tsis kam, zoo thermal shock kuj thiab stability. Lub teeb rwb thaiv tsev txheej muaj cov yam ntxwv ntawm cov thermal conductivity tsawg thiab thermal rwb thaiv tsev. Tom qab siv cov khoom siv cib sib xyaw, nws tsis tsuas yog ua tau raws li qhov yuav tsum tau ua ntawm refractory hauv ob sab phlu ntawm kiln, tab sis kuj muaj cov txiaj ntsig ntawm kev txuag hluav taws xob, txo qhov kub ntawm lub plhaub ntawm lub plhaub, txo cov roj noj, thiab txhim kho kev txuag hluav taws xob zoo.
2, Kev ua haujlwm tseem ceeb ntawm Hnav Resistant High Alumina Brick
Yam khoom | Chav tsev | TP -1 | TP -11 | Rwb thaiv tsev txheej |
Al2O3 | feem pua | Ntau dua lossis sib npaug li 77 | Ntau dua lossis sib npaug li 70 | Ntau dua lossis sib npaug li 35 |
Fe2O 3 | feem pua | Tsawg dua lossis sib npaug rau 2.0 | Tsawg dua lossis sib npaug li 2.5 | - |
Qhov ntom | g/cm3 | Ntau dua lossis sib npaug rau 2.80 | Ntau dua lossis sib npaug li 2.70 | Tsawg dua los yog sib npaug rau 1.9 |
C.C.S | Mpa | Ntau dua lossis sib npaug li 80 | Ntau dua lossis sib npaug li 70 | Ntau dua lossis sib npaug li 25 |
Refractoriness nyob rau hauv load | T0.6, degree | Ntau dua lossis sib npaug rau 1400 | Ntau dua lossis sib npaug rau 1370 | - |
Thermal shock stability | 1100 degree, dej txias, sijhawm | >12 | >12 | - |
Refractoriness | degree | 1790 | 1790 | 1660 |
3.Application: lug siv nyob rau hauv txiv qaub teb kiln, ntsug txiv qaub kiln, cement kiln, magnesium rotary kiln, thiab lwm yam
4.Main yam ntxwv:
1) Hnav Resistant High Alumina Cib yog cov qauv sib xyaw ntawm cov txheej hnyav thiab txheej txheej, uas muaj qhov kub thiab txias ua haujlwm zoo thiab ua haujlwm zoo thermal rwb thaiv tsev.
2) Cov txheej hnyav ntawm cov khoom muaj lub zog siab, zoo hnav tsis kam thiab spalling kuj. Lub teeb txheej ntawm cov khoom muaj tsawg thermal conductivity thiab zoo thermal rwb thaiv tsev kev ua tau zoo
5, Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Oman, Pakistan
6, Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom siv khoom siv dawb, siv thiab lwm yam teeb meem
Koj puas xav nrhiav tus kws tshaj lij ntawm Wear Resistant High Alumina Brick?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: ntxiv rau 86-13275332819(wechat/whatsapp tooj)
Cim npe nrov: Hnav Resistant High Alumina Cib, Tuam Tshoj, tuam ntxhab, lwm tus muag khoom, Hoobkas, siv, khoom